3D printing Nickel-based superalloy powder IN718

3D printing Nickel-based superalloy powder IN718

3D printing Nickel-based superalloy powder IN718

Detailed
3D printing Nickel-based superalloy powder IN718

 
Composition(percentage by mass)
Ni Cr Nb Mo Ti Al Cu Fe
50.0-55.0 17.0-21.0 4.75-5.25 2.80-3.30 0.65-1.15 0.20-0.80 ≤0.30 bal
 
category Alloy grades and characteristics
Alloy number: Nickel-based superalloy IN718 powder
Particle size: 15-45μm, 15-53μm, 53-120μm, 53-150μm
Morphology: Spherical or nearly spherical
Appearance: Grey
Package: Aluminum bag,Vacuum packing
Application: 3D printing metal powder
Other applications: powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

Packaging:Vacuum packing, 1kg/bag, or as your request.
Shipping:ASAP