Aluminum-based superalloy powder for 3D printing

Aluminum-based superalloy powder for 3D printing

Aluminum-based superalloy powder for 3D printing

Detailed
Aluminum-based superalloy powder for 3D printing

category Alloy grades and characteristics
Alloy number: 2219、2024、6061、AlSi7Mg(ZL101)、AlSi12(ZL102)、AlSi10Mg(ZL104)、Al-Si5Cu1Mg(ZL105)
Particle size: 0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm
Morphology: Spherical or nearly spherical
Appearance: Grey
Package: Aluminum bag,Vacuum packing
Application: 3D printing metal powder
Other applications: powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.


Alloy number Material forming process and state Mechanical property
    σb(MPa) σ0.2(MPa) δ(%)
AlSi10Mg Aluminum alloy powder Precinct laser melting/sintering heat treatment 280-350 170-220 8-18
  Forging annealing standard reference ≥300 ≥170 ≥3.5
 